In-situ TiB<sub>2</sub>/AZ31 composites were prepared by utilizing the SHS reaction of Al-Ti-B system in the molten magnesium,and the effects of external physical fields on the dispersion of TiB2 particles...In-situ TiB<sub>2</sub>/AZ31 composites were prepared by utilizing the SHS reaction of Al-Ti-B system in the molten magnesium,and the effects of external physical fields on the dispersion of TiB2 particles were investigated.The results show that high-energy ultrasonic vibration could effectively break up the particle clusters and make the TiB<sub>2</sub> particles uniformly distributed in the melt of TiB<sub>2</sub>/AZ31 composites.The compound field(high-energy ultrasonic field coupling with electromagnetic field)could not only distribute the TiB<sub>2</sub> particles into the matrix uniformly,but also make the grains ofα-Mg fine and uniform further than the ultrasonic field solo.The average grain size of as-cast TiB<sub>2</sub>/AZ31 composites was reduced from 173μm to 94μm.展开更多
基金Item Sponsored by National High Technology Research and Development Program of China[No.2009AA03Z525]Aviation Science Foundation of China[No.20095263005]
文摘In-situ TiB<sub>2</sub>/AZ31 composites were prepared by utilizing the SHS reaction of Al-Ti-B system in the molten magnesium,and the effects of external physical fields on the dispersion of TiB2 particles were investigated.The results show that high-energy ultrasonic vibration could effectively break up the particle clusters and make the TiB<sub>2</sub> particles uniformly distributed in the melt of TiB<sub>2</sub>/AZ31 composites.The compound field(high-energy ultrasonic field coupling with electromagnetic field)could not only distribute the TiB<sub>2</sub> particles into the matrix uniformly,but also make the grains ofα-Mg fine and uniform further than the ultrasonic field solo.The average grain size of as-cast TiB<sub>2</sub>/AZ31 composites was reduced from 173μm to 94μm.